HQ:NSC14/Hard/Al BS
Long Scanning, DLC Hardened, Soft Tapping Mode AFM Probe
Coating:
Hard Diamond-Like-Carbon
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
160 kHz
C
5 N/m
L
125 µm


HQ:NSC35/Hard/Al BS
AFM Probe with 3 Different Long Scanning, DLC Hardened Tapping Mode AFM Cantilevers
Coating:
Hard Diamond-Like-Carbon
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilevers: 3
1
2
3
F
205 kHz
300 kHz
150 kHz
C
8.9 N/m
16 N/m
5.4 N/m
L
110 µm
90 µm
130 µm
best bang for your buck


Tap300DLC
Diamond-Like-Carbon Coated Tapping Mode AFM Probe
Coating:
Hard Diamond-Like-Carbon
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
300 kHz
C
40 N/m
L
125 µm


BudgetComboBox
Mixed Box with 50 BudgetSensors AFM probes of your choice
Coating:
various
Tip Shape: various
Tip Shape: various


Multi75DLC
Diamond-Like-Carbon Coated Force Modulation AFM Probe
Coating:
Hard Diamond-Like-Carbon
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
75 kHz
C
3 N/m
L
225 µm


PPP-NCHAuD
Gold Coated Tapping Mode AFM Probe
Coating:
Reflective Gold
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
330 kHz
C
42 N/m
L
125 µm


PPP-RT-FMR
Standard Force Modulation AFM Probe
Coating:
Reflective Aluminum
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm


PPP-QFMR
Force Modulation AFM Probe, for UHV Conditions
Coating:
Reflective Aluminum
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm
best of the best


PPP-CONTR
Standard Contact Mode AFM Probe
Coating:
Reflective Aluminum
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
13 kHz
C
0.2 N/m
L
450 µm


ATEC-CONT
Contact Mode AFM Probe with REAL Tip Visibility
Coating:
none
Tip Shape: Visible
Tip Shape: Visible
AFM Cantilever:
F
15 kHz
C
0.2 N/m
L
450 µm
best of the best


PPP-LFMR
Standard Lateral Force Mode AFM Probes
Coating:
Reflective Aluminum
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
23 kHz
C
0.2 N/m
L
225 µm
the industry standard


CONTR
Standard Contact Mode AFM Probe
Coating:
Reflective Aluminum
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
13 kHz
C
0.2 N/m
L
450 µm


ARROW-CONTR
Contact Mode AFM Probe with Tip at the Very End of the Cantilever
Coating:
Reflective Aluminum
Tip Shape: Arrow
Tip Shape: Arrow
AFM Cantilever:
F
14 kHz
C
0.2 N/m
L
450 µm
top value


HQ:CSC17/Al BS
Standard Contact Mode AFM Probe
Coating:
Reflective Aluminum
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
13 kHz
C
0.18 N/m
L
450 µm
best bang for your buck


ContAl-G
Standard Contact Mode AFM Probe
Coating:
Reflective Aluminum
Tip Shape: Rotated
Tip Shape: Rotated
AFM Cantilever:
F
13 kHz
C
0.2 N/m
L
450 µm
best of the best


CDT-FMR
Diamond Coated, Conductive Force Modulation AFM Probe
Coating:
Diamond,Conductive Diamond
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
105 kHz
C
6.2 N/m
L
225 µm
best of the best


PPP-EFM
Electrical, Force Modulation AFM Probe
Coating:
Electrically Conductive
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
225 µm


ATEC-EFM
Electrical, Force Modulation AFM Probe with REAL Tip Visibility
Coating:
Electrically Conductive
Tip Shape: Visible
Tip Shape: Visible
AFM Cantilever:
F
85 kHz
C
2.8 N/m
L
240 µm
the industry standard


NW-CDT-FMR
Diamond Coated, Conductive Force Modulation AFM Probe
Coating:
Diamond,Conductive Diamond
Tip Shape: Standard
Tip Shape: Standard
AFM Cantilever:
F
105 kHz
C
6.2 N/m
L
225 µm


ARROW-EFM
Electrical, Force Modulation AFM Probe with Tip at the Very End of the Cantilever
Coating:
Electrically Conductive
Tip Shape: Arrow
Tip Shape: Arrow
AFM Cantilever:
F
75 kHz
C
2.8 N/m
L
240 µm